Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 30 % Show Material materials with Dehnung of 30 % |
Dehnung A50 | 20.0 °C | 25 % Show Material materials with Dehnung A50 of 25 % |
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa |
Härte, Vickers | 20.0 °C | 80 - 110 [-] Show Material materials with Härte, Vickers of 80 - 110 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 230 MPa Show Material materials with Streckgrenze Rp 0,2 of 230 MPa |
Zugfestigkeit | 20.0 °C | 320 - 380 MPa Show Material materials with Zugfestigkeit of 320 - 380 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K |
100.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | |
Schmelzpunkt | 1010 - 1030 °C Show Material materials with Schmelzpunkt of 1010 - 1030 °C | |
Wärmeleitfähigkeit | 20.0 °C | 120 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 120 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.20E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.20E+7 S/m |
spezifischer Widerstand | 20.0 °C | 8.33E-8 Ω·m Show Material materials with spezifischer Widerstand of 8.33E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.2 % Show Material materials with Phosphor of 0.2 % |
Zink | 7.5 - 10 % Show Material materials with Zink of 7.5 - 10 % |
Zinn | 1.5 - 3.5 % Show Material materials with Zinn of 1.5 - 3.5 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : good, soft brazing: very good | |
Workability | Cold forming degree between anneals: max. 90 %, general (condition): very good |