Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 10 % Show Material materials with Dehnung of 10 % | |
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation A100 | 23.0 °C | 6 % Show Material materials with Elongation A100 of 6 % | |
Härte, Brinell | 23.0 °C | 150 [-] Show Material materials with Härte, Brinell of 150 [-] | |
Härte, Vickers | 23.0 °C | 150 [-] Show Material materials with Härte, Vickers of 150 [-] | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Streckgrenze Rp 0,2 | 23.0 °C | 350 MPa Show Material materials with Streckgrenze Rp 0,2 of 350 MPa | |
Zugfestigkeit | 23.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Schmelzpunkt | 930 - 1060 °C Show Material materials with Schmelzpunkt of 930 - 1060 °C | ||
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.5 - 1.5 % Show Material materials with Blei of 0.5 - 1.5 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Phosphor | 0.01 - 0.4 % Show Material materials with Phosphor of 0.01 - 0.4 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 3.5 - 5.5 % Show Material materials with Zinn of 3.5 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : good to medium, soft brazing: very good to good | |
Workability | Cold forming degree between anneals: max. 75 %, general (condition): good to medium |