Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 45 % Show Material materials with Dehnung of 45 % |
Elastizitätsmodul | 20.0 °C | 115 GPa Show Material materials with Elastizitätsmodul of 115 GPa |
Elongation A100 | 20.0 °C | 35 % Show Material materials with Elongation A100 of 35 % |
Härte, Brinell | 20.0 °C | 90 - 120 [-] Show Material materials with Härte, Brinell of 90 - 120 [-] |
Härte, Vickers | 20.0 °C | 95 - 125 [-] Show Material materials with Härte, Vickers of 95 - 125 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 MPa |
Zugfestigkeit | 20.0 °C | 390 MPa Show Material materials with Zugfestigkeit of 390 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K |
300.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | |
Wärmeleitfähigkeit | 20.0 °C | 58 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 58 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Phosphor | 0.2 - 0.4 % Show Material materials with Phosphor of 0.2 - 0.4 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 7.5 - 8.5 % Show Material materials with Zinn of 7.5 - 8.5 % |