Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 g/cm³ Show Material materials with Dichte of 8.8 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Wanddicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 30 % Show Material materials with Dehnung of 30 % |
Härte, Brinell | 20.0 °C | 125 - 160 [-] Show Material materials with Härte, Brinell of 125 - 160 [-] |
Härte, Vickers | 20.0 °C | 130 - 165 [-] Show Material materials with Härte, Vickers of 130 - 165 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 280 MPa Show Material materials with Streckgrenze Rp 0,2 of 280 MPa |
Zugfestigkeit | 20.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.2 |
Blei | 0.1 - 0.5 % Show Material materials with Blei of 0.1 - 0.5 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Phosphor | 0.2 - 0.4 % Show Material materials with Phosphor of 0.2 - 0.4 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 7.5 - 9 % Show Material materials with Zinn of 7.5 - 9 % |