Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 45 % Show Material materials with Dehnung of 45 % |
Dehnung A50 | 20.0 °C | 36 % Show Material materials with Dehnung A50 of 36 % |
Härte, Vickers | 20.0 °C | 45 - 75 [-] Show Material materials with Härte, Vickers of 45 - 75 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 130 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 MPa |
Zugfestigkeit | 20.0 °C | 230 - 280 MPa Show Material materials with Zugfestigkeit of 230 - 280 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1050 - 1065 °C Show Material materials with Schmelzpunkt of 1050 - 1065 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Zn, total 0.1 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 94 - 96 % Show Material materials with Kupfer of 94 - 96 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : very good, soft brazing: very good | |
Workability | Cold forming degree between anneals: max. 90 %, general (condition): very good |