Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.6 g/cm³ Show Material materials with Dichte of 8.6 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 27 % Show Material materials with Dehnung of 27 % |
Elongation A100 | 20.0 °C | 20 % Show Material materials with Elongation A100 of 20 % |
Härte, Brinell | 20.0 °C | 85 - 115 [-] Show Material materials with Härte, Brinell of 85 - 115 [-] |
Härte, Vickers | 20.0 °C | 90 - 120 [-] Show Material materials with Härte, Vickers of 90 - 120 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa |
Zugfestigkeit | 20.0 °C | 310 MPa Show Material materials with Zugfestigkeit of 310 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Zn, total 0.1 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 71 - 73 % Show Material materials with Kupfer of 71 - 73 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |