Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.5 g/cm³ Show Material materials with Dichte of 8.5 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 50 % Show Material materials with Dehnung of 50 % |
Dehnung A50 | 20.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % |
Härte, Vickers | 20.0 °C | 55 - 90 [-] Show Material materials with Härte, Vickers of 55 - 90 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 170 MPa Show Material materials with Streckgrenze Rp 0,2 of 170 MPa |
Zugfestigkeit | 20.0 °C | 280 - 380 MPa Show Material materials with Zugfestigkeit of 280 - 380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Andere | Rest Zn, total 0.1 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Kupfer | 66 - 68 % Show Material materials with Kupfer of 66 - 68 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |