Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 43 % Show Material materials with Dehnung of 43 % |
Dehnung A50 | 20.0 °C | 33 % Show Material materials with Dehnung A50 of 33 % |
Härte, Vickers | 20.0 °C | 75 - 110 [-] Show Material materials with Härte, Vickers of 75 - 110 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 240 MPa Show Material materials with Streckgrenze Rp 0,2 of 240 MPa |
Zugfestigkeit | 20.0 °C | 340 - 420 MPa Show Material materials with Zugfestigkeit of 340 - 420 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 885 - 900 °C Show Material materials with Schmelzpunkt of 885 - 900 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Andere | Rest Zn, total 0.2 |
Blei | 1.6 - 2.5 % Show Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 60 - 61 % Show Material materials with Kupfer of 60 - 61 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |
Technological properties
Property | ||
---|---|---|
Brazing | hard brazing : good to medium, soft brazing: very good | |
Workability | Cold forming degree between anneals: max. 30 %, general (condition): medium |