Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 23.0 °C | 15 - 20 % Show Material materials with Dehnung of 15 - 20 % |
Härte, Brinell | 23.0 °C | 80 [-] Show Material materials with Härte, Brinell of 80 [-] |
Härte, Vickers | 23.0 °C | 85 [-] Show Material materials with Härte, Vickers of 85 [-] |
Streckgrenze Rp 0,2 | 23.0 °C | 120 - 140 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 - 140 MPa |
Zugfestigkeit | 23.0 °C | 350 - 360 MPa Show Material materials with Zugfestigkeit of 350 - 360 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | Rest Zn, total 0.2 |
Blei | 1.6 - 2.5 % Show Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 - 0.5 % Show Material materials with Zinn of 0.2 - 0.5 % |