Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.5 g/cm³ Show Material materials with Dichte of 8.5 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Wanddicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 50 % Show Material materials with Dehnung of 50 % |
Härte, Brinell | 20.0 °C | 60 - 80 [-] Show Material materials with Härte, Brinell of 60 - 80 [-] |
Härte, Vickers | 20.0 °C | 65 - 85 [-] Show Material materials with Härte, Vickers of 65 - 85 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 115 MPa Show Material materials with Streckgrenze Rp 0,2 of 115 MPa |
Zugfestigkeit | 20.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.5 |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 81 - 84 % Show Material materials with Kupfer of 81 - 84 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 0.8 - 1.4 % Show Material materials with Nickel of 0.8 - 1.4 % |
Silizium | 0.8 - 1.3 % Show Material materials with Silizium of 0.8 - 1.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |