Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Dicke |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 30 % Show Material materials with Dehnung of 30 % |
Härte, Vickers | 20.0 °C | 70 - 105 [-] Show Material materials with Härte, Vickers of 70 - 105 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 90 MPa Show Material materials with Streckgrenze Rp 0,2 of 90 MPa |
Zugfestigkeit | 20.0 °C | 330 MPa Show Material materials with Zugfestigkeit of 330 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.8 - 2.3 % Show Material materials with Aluminium of 1.8 - 2.3 % |
Andere | Rest Zn, total 0.3 |
Arsen | 0.02 - 0.06 % Show Material materials with Arsen of 0.02 - 0.06 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.07 % Show Material materials with Eisen of 0.07 % |
Kupfer | 76 - 79 % Show Material materials with Kupfer of 76 - 79 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |