Chemical properties
Property | Value |
---|---|
Aluminium | 1.8 - 2.3 % Show Material materials with Aluminium of 1.8 - 2.3 % |
Andere | Rest Zn, total 0.1 |
Arsen | 0.02 - 0.035 % Show Material materials with Arsen of 0.02 - 0.035 % |
Blei | 0.07 % Show Material materials with Blei of 0.07 % |
Eisen | 0.07 % Show Material materials with Eisen of 0.07 % |
Kupfer | 76 - 79 % Show Material materials with Kupfer of 76 - 79 % |
Magnesium | 5E-3 % Show Material materials with Magnesium of 5E-3 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |