Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 8 % Show Material materials with Dehnung of 8 % |
Härte, Brinell | 20.0 °C | 190 [-] Show Material materials with Härte, Brinell of 190 [-] |
Härte, Vickers | 20.0 °C | 200 [-] Show Material materials with Härte, Vickers of 200 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 540 MPa Show Material materials with Streckgrenze Rp 0,2 of 540 MPa |
Zugfestigkeit | 20.0 °C | 780 MPa Show Material materials with Zugfestigkeit of 780 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 5 - 6 % Show Material materials with Aluminium of 5 - 6 % |
Andere | Rest Zn, total 0.2 |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 2 - 3.5 % Show Material materials with Eisen of 2 - 3.5 % |
Kupfer | 63 - 65 % Show Material materials with Kupfer of 63 - 65 % |
Mangan | 3.5 - 5 % Show Material materials with Mangan of 3.5 - 5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |