Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Härte, Brinell | 20.0 °C | 170 - 200 [-] Show Material materials with Härte, Brinell of 170 - 200 [-] |
Härte, Vickers | 20.0 °C | 180 - 210 [-] Show Material materials with Härte, Vickers of 180 - 210 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 360 MPa Show Material materials with Streckgrenze Rp 0,2 of 360 MPa |
Zugfestigkeit | 20.0 °C | 620 MPa Show Material materials with Zugfestigkeit of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 4 - 5 % Show Material materials with Aluminium of 4 - 5 % |
Andere | Rest Zn, total 0.3 |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 0.5 - 3 % Show Material materials with Eisen of 0.5 - 3 % |
Kupfer | 65 - 68 % Show Material materials with Kupfer of 65 - 68 % |
Mangan | 0.5 - 3 % Show Material materials with Mangan of 0.5 - 3 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Zinn | 0.9 - 1.3 % Show Material materials with Zinn of 0.9 - 1.3 % |