Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % |
Härte, Brinell | 20.0 °C | 100 [-] Show Material materials with Härte, Brinell of 100 [-] |
Härte, Vickers | 20.0 °C | 105 [-] Show Material materials with Härte, Vickers of 105 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 200 MPa |
Zugfestigkeit | 20.0 °C | 440 MPa Show Material materials with Zugfestigkeit of 440 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Material materials with Aluminium of 0.3 - 1.3 % |
Andere | Rest Zn, total 0.3 |
Blei | 0.2 - 0.8 % Show Material materials with Blei of 0.2 - 0.8 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Mangan | 0.8 - 1.8 % Show Material materials with Mangan of 0.8 - 1.8 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.2 - 0.8 % Show Material materials with Silizium of 0.2 - 0.8 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |