Chemical properties
Property | Value |
---|---|
Aluminium | 0.6 % Show Material materials with Aluminium of 0.6 % |
Andere | Rest Zn, total 0.5 |
Blei | 0.7 - 1.8 % Show Material materials with Blei of 0.7 - 1.8 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 56 - 59 % Show Material materials with Kupfer of 56 - 59 % |
Mangan | 0.5 - 1.8 % Show Material materials with Mangan of 0.5 - 1.8 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |