Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.3 g/cm³ Show Material materials with Dichte of 8.3 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Durchmesser |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Härte, Brinell | 20.0 °C | 110 - 140 [-] Show Material materials with Härte, Brinell of 110 - 140 [-] |
Härte, Vickers | 20.0 °C | 115 - 145 [-] Show Material materials with Härte, Vickers of 115 - 145 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 270 MPa Show Material materials with Streckgrenze Rp 0,2 of 270 MPa |
Zugfestigkeit | 20.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | Rest Zn, total 0.4 |
Blei | 0.5 % Show Material materials with Blei of 0.5 % |
Eisen | 0.5 - 1.5 % Show Material materials with Eisen of 0.5 - 1.5 % |
Kupfer | 56.5 - 58.5 % Show Material materials with Kupfer of 56.5 - 58.5 % |
Mangan | 1 - 2 % Show Material materials with Mangan of 1 - 2 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |