Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, total 0.50 |
Bismut | 0.03 % Show Material materials with Bismut of 0.03 % |
Blei | 1.5 % Show Material materials with Blei of 1.5 % |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.1 % Show Material materials with Schwefel of 0.1 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zink | 1.75 - 2.75 % Show Material materials with Zink of 1.75 - 2.75 % |
Zinn | 9.5 - 10.5 % Show Material materials with Zinn of 9.5 - 10.5 % |