Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 2 % Show Material materials with Aluminium of 0.5 - 2 % |
Blei | 0.4 % Show Material materials with Blei of 0.4 % |
Eisen | 0.5 - 3.5 % Show Material materials with Eisen of 0.5 - 3.5 % |
Kupfer | 55 - 60 % Show Material materials with Kupfer of 55 - 60 % |
Mangan | 0.1 - 1.5 % Show Material materials with Mangan of 0.1 - 1.5 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 30 - 42 % Show Material materials with Zink of 30 - 42 % |
Zinn | 1 % Show Material materials with Zinn of 1 % |