Chemical properties
Property | Value |
---|---|
Aluminium | 3 - 5 % Show Material materials with Aluminium of 3 - 5 % |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 2 - 4 % Show Material materials with Eisen of 2 - 4 % |
Kupfer | 60 - 65 % Show Material materials with Kupfer of 60 - 65 % |
Mangan | 2.5 - 5 % Show Material materials with Mangan of 2.5 - 5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zink | 22 - 28 % Show Material materials with Zink of 22 - 28 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |