Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Andere | Rest Zn, total 1.5 |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Bismut | 3E-3 % Show Material materials with Bismut of 3E-3 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.6 % Show Material materials with Eisen of 0.6 % |
Kupfer | 79 - 81 % Show Material materials with Kupfer of 79 - 81 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Silizium | 2.5 - 4 % Show Material materials with Silizium of 2.5 - 4 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |