Chemical properties
Property | Value |
---|---|
Aluminium | 2.5 - 3.5 % Show Material materials with Aluminium of 2.5 - 3.5 % |
Andere | Rest Zn, total 0.9 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Bismut | 3E-3 % Show Material materials with Bismut of 3E-3 % |
Blei | 0.1 % Show Material materials with Blei of 0.1 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 57 - 60 % Show Material materials with Kupfer of 57 - 60 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |