Chemical properties
Property | Value |
---|---|
Aluminium | 1.6 - 2.2 % Show Material materials with Aluminium of 1.6 - 2.2 % |
Andere | Rest Zn, total 0.5 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 73 - 76 % Show Material materials with Kupfer of 73 - 76 % |
Mangan | 0.3 - 0.7 % Show Material materials with Mangan of 0.3 - 0.7 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Silizium | 0.3 - 0.7 % Show Material materials with Silizium of 0.3 - 0.7 % |