Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimon | 0.5 % Show Material materials with Antimon of 0.5 % |
Blei | 16 - 22 % Show Material materials with Blei of 16 - 22 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 70 - 76 % Show Material materials with Kupfer of 70 - 76 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Silizium | 5E-3 % Show Material materials with Silizium of 5E-3 % |
Zink | 1 % Show Material materials with Zink of 1 % |