Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.3 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Arsen | 0.025 - 0.06 % Show Material materials with Arsen of 0.025 - 0.06 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.03 % Show Material materials with Blei of 0.03 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 67 - 70 % Show Material materials with Kupfer of 67 - 70 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |