Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.5 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.6 - 1 % Show Material materials with Blei of 0.6 - 1 % |
Eisen | 0.15 % Show Material materials with Eisen of 0.15 % |
Kupfer | 59 - 61 % Show Material materials with Kupfer of 59 - 61 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |