Chemical properties
Property | Value |
---|---|
Andere | Cu+Ag > 99.97 |
Antimon | 1E-3 % Show Material materials with Antimon of 1E-3 % |
Arsen | 1E-3 % Show Material materials with Arsen of 1E-3 % |
Bismut | 5E-4 % Show Material materials with Bismut of 5E-4 % |
Blei | 2E-3 % Show Material materials with Blei of 2E-3 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Nickel | 1E-3 % Show Material materials with Nickel of 1E-3 % |
Phosphor | 1E-3 % Show Material materials with Phosphor of 1E-3 % |
Sauerstoff | 0.02 % Show Material materials with Sauerstoff of 0.02 % |
Schwefel | 2E-3 % Show Material materials with Schwefel of 2E-3 % |
Silber | 2E-3 % Show Material materials with Silber of 2E-3 % |
Zink | 1E-3 % Show Material materials with Zink of 1E-3 % |
Zinn | 1E-3 % Show Material materials with Zinn of 1E-3 % |