Chemical properties
Property | Value |
---|---|
Antimon | 4E-4 % Show Material materials with Antimon of 4E-4 % |
Arsen | 5E-4 % Show Material materials with Arsen of 5E-4 % |
Blei | 5E-4 % Show Material materials with Blei of 5E-4 % |
Eisen | 1E-3 % Show Material materials with Eisen of 1E-3 % |
Sauerstoff | 0.01 % Show Material materials with Sauerstoff of 0.01 % |
Schwefel | 1.5E-3 % Show Material materials with Schwefel of 1.5E-3 % |
Silber | 2E-3 % Show Material materials with Silber of 2E-3 % |