Chemical properties
Property | Value |
---|---|
Andere | Cu+Ag > 99.90 |
Antimon | 2E-3 % Show Material materials with Antimon of 2E-3 % |
Arsen | 2E-3 % Show Material materials with Arsen of 2E-3 % |
Bismut | 1E-3 % Show Material materials with Bismut of 1E-3 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Phosphor | 0.01 - 0.04 % Show Material materials with Phosphor of 0.01 - 0.04 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Zink | 5E-3 % Show Material materials with Zink of 5E-3 % |
Zinn | 2E-3 % Show Material materials with Zinn of 2E-3 % |