Chemical properties
Property | Value |
---|---|
Andere | Cu+Ag > 99.50 |
Antimon | 0.05 % Show Material materials with Antimon of 0.05 % |
Arsen | 0.01 % Show Material materials with Arsen of 0.01 % |
Bismut | 3E-3 % Show Material materials with Bismut of 3E-3 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.05 % Show Material materials with Eisen of 0.05 % |
Nickel | 0.2 % Show Material materials with Nickel of 0.2 % |
Sauerstoff | 0.08 % Show Material materials with Sauerstoff of 0.08 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Zinn | 0.05 % Show Material materials with Zinn of 0.05 % |