Chemical properties
Property | Value |
---|---|
Andere | Rest Zn, total 0.3 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.8 - 1.2 % Show Material materials with Blei of 0.8 - 1.2 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 62 - 64 % Show Material materials with Kupfer of 62 - 64 % |
Nickel | 0.5 - 0.8 % Show Material materials with Nickel of 0.5 - 0.8 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |