Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.10 |
Antimon | 2E-3 % Show Material materials with Antimon of 2E-3 % |
Arsen | 2E-3 % Show Material materials with Arsen of 2E-3 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Kohlenstoff | 2E-3 % Show Material materials with Kohlenstoff of 2E-3 % |
Nickel | 0.52 - 0.58 % Show Material materials with Nickel of 0.52 - 0.58 % |
Phosphor | 2E-3 % Show Material materials with Phosphor of 2E-3 % |
Schwefel | 5E-3 % Show Material materials with Schwefel of 5E-3 % |
Silizium | 2E-3 % Show Material materials with Silizium of 2E-3 % |