Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 1.3 |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 24 - 26 % Show Material materials with Nickel of 24 - 26 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |