Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.90 |
Antimon | 2E-3 % Show Material materials with Antimon of 2E-3 % |
Arsen | 5E-3 % Show Material materials with Arsen of 5E-3 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 0.02 % Show Material materials with Blei of 0.02 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kohlenstoff | 0.05 % Show Material materials with Kohlenstoff of 0.05 % |
Magnesium | 0.03 % Show Material materials with Magnesium of 0.03 % |
Mangan | 11.5 - 13.5 % Show Material materials with Mangan of 11.5 - 13.5 % |
Nickel | 2.5 - 3.5 % Show Material materials with Nickel of 2.5 - 3.5 % |
Phosphor | 5E-3 % Show Material materials with Phosphor of 5E-3 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |