Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.95 g/cm³ Show Material materials with Dichte of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 156 GPa Show Material materials with Elastizitätsmodul of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Schmelzpunkt | 915 - 1240 °C Show Material materials with Schmelzpunkt of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Spezifische Wärmekapazität | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.7 |
Antimon | 5E-3 % Show Material materials with Antimon of 5E-3 % |
Arsen | 0.01 % Show Material materials with Arsen of 0.01 % |
Bismut | 2E-3 % Show Material materials with Bismut of 2E-3 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 1 - 1.4 % Show Material materials with Eisen of 1 - 1.4 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 0.3 - 0.8 % Show Material materials with Mangan of 0.3 - 0.8 % |
Nickel | 5 - 6.5 % Show Material materials with Nickel of 5 - 6.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.15 % Show Material materials with Silizium of 0.15 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |