Chemical properties
Property | Value |
---|---|
Andere | Rest Cu, total 0.10 |
Antimon | 2E-3 % Show Material materials with Antimon of 2E-3 % |
Arsen | 2E-3 % Show Material materials with Arsen of 2E-3 % |
Bismut | 1E-3 % Show Material materials with Bismut of 1E-3 % |
Blei | 5E-3 % Show Material materials with Blei of 5E-3 % |
Eisen | 5E-3 % Show Material materials with Eisen of 5E-3 % |
Nickel | 2E-3 % Show Material materials with Nickel of 2E-3 % |
Sauerstoff | 0.04 % Show Material materials with Sauerstoff of 0.04 % |
Schwefel | 4E-3 % Show Material materials with Schwefel of 4E-3 % |
Silber | 0.05 - 0.25 % Show Material materials with Silber of 0.05 - 0.25 % |
Zink | 3E-3 % Show Material materials with Zink of 3E-3 % |
Zinn | 2E-3 % Show Material materials with Zinn of 2E-3 % |