Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Andere | Rest Cu, total 0.20 |
Blei | 0.5 % Show Material materials with Blei of 0.5 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Phosphor | 0.25 - 0.6 % Show Material materials with Phosphor of 0.25 - 0.6 % |
Schwefel | 0.1 % Show Material materials with Schwefel of 0.1 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 11.2 - 13 % Show Material materials with Zinn of 11.2 - 13 % |