Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.77 g/cm³ Show Material materials with Dichte of 2.77 g/cm³ | T62 | WL 3.1354 | Strip, Sheet, Plate |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Biegewinkel 180° | 4.0 °/t Show Material materials with Biegewinkel 180° of 4.0 °/t | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Elastizitätsmodul | 72.4 GPa Show Material materials with Elastizitätsmodul of 72.4 GPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Härte, Brinell | 120.0 [-] Show Material materials with Härte, Brinell of 120.0 [-] | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | |||
Schubmodule | 27.6 GPa Show Material materials with Schubmodule of 27.6 GPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
Zugfestigkeit | 415.0 MPa Show Material materials with Zugfestigkeit of 415.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate | |
435.0 MPa Show Material materials with Zugfestigkeit of 435.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
440.0 MPa Show Material materials with Zugfestigkeit of 440.0 MPa | T62 | WL 3.1354 | Strip, Sheet, Plate |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 2.1499999999999997e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1499999999999997e-05 1/K | T62 | WL 3.1354 | Strip, Sheet, Plate | |
100 °C | 2.1499999999999997e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1499999999999997e-05 1/K | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
Schmelzpunkt | 500.0 - 640.0 °C Show Material materials with Schmelzpunkt of 500.0 - 640.0 °C | T62 | WL 3.1354 | Strip, Sheet, Plate | ||
Spezifische Wärmekapazität | 816.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 816.0 - 963.0 J/(kg·K) | Typical for Wrought 2000 Series Aluminium | ||||
Wärmeleitfähigkeit | 109.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 109.0 - 160.0 W/(m·K) | T62 | WL 3.1354 | Strip, Sheet, Plate |
Elektrisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Elektrische Leitfähigkeit | 15000000.0 - 23000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 15000000.0 - 23000000.0 S/m | T62 | WL 3.1354 | Strip, Sheet, Plate |
spezifischer Widerstand | 4.35e-08 - 6.67e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.35e-08 - 6.67e-08 Ω·m | T62 | WL 3.1354 | Strip, Sheet, Plate |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chrom | 0.1 % Show Material materials with Chrom of 0.1 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Eisen | 0.50 % Show Material materials with Eisen of 0.50 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Kupfer | 3.8 - 4.9 % Show Material materials with Kupfer of 3.8 - 4.9 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Mangan | 0.3 - 0.9 % Show Material materials with Mangan of 0.3 - 0.9 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Zink | 0.25 % Show Material materials with Zink of 0.25 % | T62 | WL 3.1354 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Moderate Workability |