Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 180 - 270 MPa Show Supplier Material materials with Biegefestigkeit of 180 - 270 MPa |
Elastizitätsmodul | 23.0 °C | 150 - 160 GPa Show Supplier Material materials with Elastizitätsmodul of 150 - 160 GPa |
Zugfestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 100 °C Show Supplier Material materials with Max. Betriebstemperatur of 100 °C |
Magnetisch
Property | Temperature | Value | Comment |
---|---|---|---|
Intrinsic coercivity | 23.0 °C | 1.11E+6 A/m Show Supplier Material materials with Intrinsic coercivity of 1.11E+6 A/m | min |
Koerzitivfeldstärke | 23.0 °C | 939000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 939000 A/m | min |
Maximalenergieprodukt | 23.0 °C | 303 - 318 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 303 - 318 kJ/m³ | |
Remanenz | 23.0 °C | 1.26 - 1.29 T Show Supplier Material materials with Remanenz of 1.26 - 1.29 T | |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.12 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.12 %/ °C | |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | 0.65 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of 0.65 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Motors, Sensors | |
Other | Mid grade temperature rated NdFeB |