Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.3 g/cm³ Show Supplier Material materials with Dichte of 7.3 g/cm³ |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 550 °C Show Supplier Material materials with Max. Betriebstemperatur of 550 °C |
Magnetisch
Property | Temperature | Value |
---|---|---|
Intrinsic coercivity | 23.0 °C | 51000 A/m Show Supplier Material materials with Intrinsic coercivity of 51000 A/m |
Koerzitivfeldstärke | 23.0 °C | 51000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 51000 A/m |
Maximalenergieprodukt | 23.0 °C | 40 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 40 kJ/m³ |
Remanenz | 23.0 °C | 1.25 T Show Supplier Material materials with Remanenz of 1.25 T |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.02 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.02 %/ °C |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | 0.03 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of 0.03 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Holding, Instruments | |
Other | Cast magnet material, great for holding devices |