Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Dichte of 8.3 g/cm³ |
Mechanisch
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 250 °C Show Supplier Material materials with Max. Betriebstemperatur of 250 °C |
Magnetisch
Property | Temperature | Value |
---|---|---|
Intrinsic coercivity | 23.0 °C | 1.43E+6 A/m Show Supplier Material materials with Intrinsic coercivity of 1.43E+6 A/m |
Koerzitivfeldstärke | 23.0 °C | 676000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 676000 A/m |
Maximalenergieprodukt | 23.0 °C | 175 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 175 kJ/m³ |
Remanenz | 23.0 °C | 0.93 T Show Supplier Material materials with Remanenz of 0.93 T |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.04 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.04 %/ °C |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | 0.03 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of 0.03 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Medical | |
Other | Highest temperature rated magnet, no need for plating |