Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 90 - 150 MPa Show Supplier Material materials with Biegefestigkeit of 90 - 150 MPa |
Elastizitätsmodul | 23.0 °C | 150 GPa Show Supplier Material materials with Elastizitätsmodul of 150 GPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 350 °C Show Supplier Material materials with Max. Betriebstemperatur of 350 °C |
Magnetisch
Property | Temperature | Value |
---|---|---|
Intrinsic coercivity | 23.0 °C | 1.19E+6 A/m Show Supplier Material materials with Intrinsic coercivity of 1.19E+6 A/m |
Koerzitivfeldstärke | 23.0 °C | 756000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 756000 A/m |
Maximalenergieprodukt | 23.0 °C | 223 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 223 kJ/m³ |
Remanenz | 23.0 °C | 1.07 T Show Supplier Material materials with Remanenz of 1.07 T |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.05 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.05 %/ °C |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | 0.08 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of 0.08 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace, Medical | |
Other | Strongest SmCo material |