Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 4.8 - 5 g/cm³ Show Supplier Material materials with Dichte of 4.8 - 5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Biegefestigkeit of 55 MPa |
Elastizitätsmodul | 23.0 °C | 150 GPa Show Supplier Material materials with Elastizitätsmodul of 150 GPa |
Zugfestigkeit | 23.0 °C | 20 - 50 MPa Show Supplier Material materials with Zugfestigkeit of 20 - 50 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 350 °C Show Supplier Material materials with Max. Betriebstemperatur of 350 °C |
Magnetisch
Property | Temperature | Value |
---|---|---|
Intrinsic coercivity | 23.0 °C | 243000 - 275000 A/m Show Supplier Material materials with Intrinsic coercivity of 243000 - 275000 A/m |
Koerzitivfeldstärke | 23.0 °C | 239000 - 271000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 239000 - 271000 A/m |
Maximalenergieprodukt | 23.0 °C | 27.1 - 31.2 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 27.1 - 31.2 kJ/m³ |
Remanenz | 23.0 °C | 0.38 - 0.41 T Show Supplier Material materials with Remanenz of 0.38 - 0.41 T |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.18 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.18 %/ °C |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | -0.04 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of -0.04 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Motors, Loudspeakers | |
Other | Most common and least expensive magnet in industry |