Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 5.6 - 6 g/cm³ Show Supplier Material materials with Dichte of 5.6 - 6 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 0.7 - 1 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 - 1 GPa |
Zugfestigkeit | 23.0 °C | 37 MPa Show Supplier Material materials with Zugfestigkeit of 37 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 120 °C Show Supplier Material materials with Max. Betriebstemperatur of 120 °C |
Magnetisch
Property | Temperature | Value |
---|---|---|
Intrinsic coercivity | 23.0 °C | 680000 - 800000 A/m Show Supplier Material materials with Intrinsic coercivity of 680000 - 800000 A/m |
Koerzitivfeldstärke | 23.0 °C | 440000 - 480000 A/m Show Supplier Material materials with Koerzitivfeldstärke of 440000 - 480000 A/m |
Maximalenergieprodukt | 23.0 °C | 80 - 88 kJ/m³ Show Supplier Material materials with Maximalenergieprodukt of 80 - 88 kJ/m³ |
Remanenz | 23.0 °C | 0.68 - 0.71 T Show Supplier Material materials with Remanenz of 0.68 - 0.71 T |
Reversible Remanenz des Temperaturkoeffizienten | 23.0 °C | 0.11 %/ °C Show Supplier Material materials with Reversible Remanenz des Temperaturkoeffizienten of 0.11 %/ °C |
Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke | 23.0 °C | 0.39 %/ °C Show Supplier Material materials with Umkehrbare Temperaturkoeffizient-Koerzitivfeldstärke of 0.39 %/ °C |
Technological properties
Property | ||
---|---|---|
Application areas | Small DC Motors | |
Other | NdFeB that is bonded for rings and special shapes |