Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.71 g/cm³ Show Supplier Material materials with Dichte of 2.71 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 0.3 mm Show Supplier Material materials with Dicke of 0.2 - 0.3 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegewinkel 90° | 23.0 °C | 1 °/t Show Supplier Material materials with Biegewinkel 90° of 1 °/t | according to EN 485-2 |
Dehnung A50 | 23.0 °C | 1 % Show Supplier Material materials with Dehnung A50 of 1 % | according to EN 485-2 |
Elastizitätsmodul | 23.0 °C | 69 GPa Show Supplier Material materials with Elastizitätsmodul of 69 GPa | |
Härte, HBW | 23.0 °C | 47 [-] Show Supplier Material materials with Härte, HBW of 47 [-] | according to EN 485-2 |
Schubmodule | 23.0 °C | 26 GPa Show Supplier Material materials with Schubmodule of 26 GPa | |
Streckgrenze | 23.0 °C | 155 MPa Show Supplier Material materials with Streckgrenze of 155 MPa | according to EN 485-2 |
Zugfestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Zugfestigkeit of 165 MPa | according to EN 485-2 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 220 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 220 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 2.82E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.82E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 0.01 % Show Supplier Material materials with Chrom of 0.01 % |
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % |
Magnesium | 0.3 - 0.4 % Show Supplier Material materials with Magnesium of 0.3 - 0.4 % |
Mangan | 0.05 % Show Supplier Material materials with Mangan of 0.05 % |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % |
Zink | 0.07 % Show Supplier Material materials with Zink of 0.07 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Lithography | |
Brazing | Excellent | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |