Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Dichte of 2.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 3 mm Show Supplier Material materials with Dicke of 0.2 - 3 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegewinkel 180° | 23.0 °C | 0 °/t Show Supplier Material materials with Biegewinkel 180° of 0 °/t |
Biegewinkel 90° | 23.0 °C | 0 °/t Show Supplier Material materials with Biegewinkel 90° of 0 °/t |
Dehnung A50 | 23.0 °C | 20 % Show Supplier Material materials with Dehnung A50 of 20 % |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Härte, HBW | 23.0 °C | 20 [-] Show Supplier Material materials with Härte, HBW of 20 [-] |
Schubmodule | 23.0 °C | 26.5 GPa Show Supplier Material materials with Schubmodule of 26.5 GPa |
Streckgrenze | 23.0 °C | 20 MPa Show Supplier Material materials with Streckgrenze of 20 MPa |
Zugfestigkeit | 23.0 °C | 65 - 95 MPa Show Supplier Material materials with Zugfestigkeit of 65 - 95 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 138 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.03 % Show Supplier Material materials with Andere of 0.03 % |
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % |
Magnesium | 0.05 % Show Supplier Material materials with Magnesium of 0.05 % |
Mangan | 0.05 % Show Supplier Material materials with Mangan of 0.05 % |
Silizium | 0.25 % Show Supplier Material materials with Silizium of 0.25 % |
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % |
Zink | 0.07 % Show Supplier Material materials with Zink of 0.07 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Lithography; Cable Wrapping: Electric cable wrapping; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, rotor hub, stairs; Cosmetics: Cosmetics pieces; Automotive Trim: Interior Trim, Marque Badges; Components: Heat shields, General Transportation | |
Brazing | Excellent | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |