Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Dichte of 2.7 g/cm³ |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.3E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 235 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 235 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 2.79E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 2.79E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.01 % Show Supplier Material materials with Andere of 0.01 % |
Eisen | 0.12 % Show Supplier Material materials with Eisen of 0.12 % |
Gallium | 0.03 % Show Supplier Material materials with Gallium of 0.03 % |
Kupfer | 0.03 % Show Supplier Material materials with Kupfer of 0.03 % |
Magnesium | 0.02 % Show Supplier Material materials with Magnesium of 0.02 % |
Mangan | 0.02 % Show Supplier Material materials with Mangan of 0.02 % |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % |
Titan | 0.02 % Show Supplier Material materials with Titan of 0.02 % |
Vanadium | 0.05 % Show Supplier Material materials with Vanadium of 0.05 % |
Zink | 0.03 % Show Supplier Material materials with Zink of 0.03 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Excellent | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Lighting: Anodizing Quality, Lacquering quality; Electronic devices: Housing of devices; Tubes: Industrial tubes, Flexible tube, Pipes; Insulation; Solar: Solar collectors, Photovoltaic panels; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Cosmetics: Cosmetic pieces; Automotive trim: Interior trim, Windows frame, Marque badges | |
Corrosion properties | Excellent | |
Welding | Excellent | |
Workability | Excellent |