Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Dichte of 2.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 60 - 400 mm Show Supplier Material materials with Dicke of 60 - 400 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 10 % Show Supplier Material materials with Dehnung A50 of 10 % |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Schubmodule | 23.0 °C | 26.5 GPa Show Supplier Material materials with Schubmodule of 26.5 GPa |
Streckgrenze | 23.0 °C | 65 MPa Show Supplier Material materials with Streckgrenze of 65 MPa |
Zugfestigkeit | 23.0 °C | 60 - 105 MPa Show Supplier Material materials with Zugfestigkeit of 60 - 105 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 138 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.9E-8 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | |
Eisen | 1 % Show Supplier Material materials with Eisen of 1 % | Si + Fe |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % | |
Mangan | 0.05 % Show Supplier Material materials with Mangan of 0.05 % | |
Silizium | 1 % Show Supplier Material materials with Silizium of 1 % | Si + Fe |
Titan | 0.05 % Show Supplier Material materials with Titan of 0.05 % | |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Very Good | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels; Roofing: Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels; Electronic devices: Housing of devices; Heat exchangers: Fins; Cable wrapping: Electric cable wrapping; Insulation; Solar: Solar collectors; Semi-rigid and corrugated: Smooth wall | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Excellent | |
Workability | Excellent |