Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.69 g/cm³ Show Supplier Material materials with Dichte of 2.69 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 3 mm Show Supplier Material materials with Dicke of 0.2 - 3 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegewinkel 180° | 23.0 °C | 0 °/t Show Supplier Material materials with Biegewinkel 180° of 0 °/t |
Biegewinkel 90° | 23.0 °C | 0 °/t Show Supplier Material materials with Biegewinkel 90° of 0 °/t |
Elastizitätsmodul | 23.0 °C | 70 GPa Show Supplier Material materials with Elastizitätsmodul of 70 GPa |
Schubmodule | 23.0 °C | 26.5 GPa Show Supplier Material materials with Schubmodule of 26.5 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 138 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 138 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.9E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.9E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Andere | 0.1 % Show Supplier Material materials with Andere of 0.1 % |
Chrom | 0.01 % Show Supplier Material materials with Chrom of 0.01 % |
Eisen | 0.4 % Show Supplier Material materials with Eisen of 0.4 % |
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % |
Mangan | 0.01 % Show Supplier Material materials with Mangan of 0.01 % |
Silizium | 0.1 % Show Supplier Material materials with Silizium of 0.1 % |
Zink | 0.05 % Show Supplier Material materials with Zink of 0.05 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good (For surface protection only) | |
Application areas | Conductors; rods for the manufacture of aluminium conductor wires. | |
Brazing | Excellent | |
Corrosion properties | Very Good | |
Welding | Very Good | |
Workability | Very Good |