Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.72 g/cm³ Show Supplier Material materials with Dichte of 2.72 g/cm³ |
Abmessung
Property | Value |
---|---|
Dicke | 0.2 - 1 mm Show Supplier Material materials with Dicke of 0.2 - 1 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegewinkel 180° | 23.0 °C | 2 °/t Show Supplier Material materials with Biegewinkel 180° of 2 °/t |
Biegewinkel 90° | 23.0 °C | 0.5 °/t Show Supplier Material materials with Biegewinkel 90° of 0.5 °/t |
Dehnung A50 | 23.0 °C | 1 % Show Supplier Material materials with Dehnung A50 of 1 % |
Elastizitätsmodul | 23.0 °C | 68.6 GPa Show Supplier Material materials with Elastizitätsmodul of 68.6 GPa |
Härte, HBW | 23.0 °C | 66 [-] Show Supplier Material materials with Härte, HBW of 66 [-] |
Schubmodule | 23.0 °C | 26 GPa Show Supplier Material materials with Schubmodule of 26 GPa |
Streckgrenze | 23.0 °C | 170 MPa Show Supplier Material materials with Streckgrenze of 170 MPa |
Zugfestigkeit | 23.0 °C | 190 - 265 MPa Show Supplier Material materials with Zugfestigkeit of 190 - 265 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.4E-5 1/K | 20-100°C |
Wärmeleitfähigkeit | 23.0 °C | 163 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 163 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 4.1E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 4.1E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Eisen | 0.7 % Show Supplier Material materials with Eisen of 0.7 % |
Kupfer | 0.25 % Show Supplier Material materials with Kupfer of 0.25 % |
Magnesium | 0.8 - 1.3 % Show Supplier Material materials with Magnesium of 0.8 - 1.3 % |
Mangan | 1 - 1.5 % Show Supplier Material materials with Mangan of 1 - 1.5 % |
Silizium | 0.3 % Show Supplier Material materials with Silizium of 0.3 % |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % |
Technological properties
Property | ||
---|---|---|
Anodizing | Good (For surface protection only) | |
Application areas | Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Food can: Body, Lids; Semi-rigid and corrugated: Smooth wall | |
Brazing | Very Good | |
Corrosion properties | Good | |
Welding | Very Good | |
Workability | Good |